S. Tekeli Et Al. , "High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression," CERAMICS INTERNATIONAL , vol.33, no.5, pp.869-874, 2007
Tekeli, S. Et Al. 2007. High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression. CERAMICS INTERNATIONAL , vol.33, no.5 , 869-874.
Tekeli, S., Chen, T., Nagayama, H., Sakuma, T., & Mecartney, M. L., (2007). High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression. CERAMICS INTERNATIONAL , vol.33, no.5, 869-874.
Tekeli, SÜLEYMAN Et Al. "High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression," CERAMICS INTERNATIONAL , vol.33, no.5, 869-874, 2007
Tekeli, SÜLEYMAN Et Al. "High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression." CERAMICS INTERNATIONAL , vol.33, no.5, pp.869-874, 2007
Tekeli, S. Et Al. (2007) . "High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression." CERAMICS INTERNATIONAL , vol.33, no.5, pp.869-874.
@article{article, author={SÜLEYMAN TEKELİ Et Al. }, title={High-temperature deformation behaviour of TiO2-doped 2 mol.% Y2O3-stabilized ZrO2 (8Y-CSZ) under tension and compression}, journal={CERAMICS INTERNATIONAL}, year=2007, pages={869-874} }