Kimyasal yöntemle poli(alkilanilin)lerin sentezi; iletken polimerlerle bazı kompozitlerin hazırlanması ve özelliklerinin incelenmesi


Thesis Type: Postgraduate

Institution Of The Thesis: Gazi University, Fen Bilimleri Enstitüsü, KİMYA ANABİLİM DALI, Turkey

Approval Date: 2003

Thesis Language: Turkish

Student: DERYA ŞAHİN

Supervisor: BEKİR SARI

Abstract:

uı CHEMICAL SYNTHESIS OF POLY(ALKYLANILINES); PREPARATION OF THEIR SOME COMPOSITES WITH VARIOUS CONDUCTING POLYMERS AND CHARACTERIZATION (M.Sc. Thesis) Derya ŞAHİN GAZİ UNIVERSITY INSTITUTE OF SCIENCE AND TECHNOLOGY June, 2003 ABSTRACT In this study, conductivite polymers of alkylanilines, pyrrole and their conducting composites were synthesized by chemical method. Among the poly(alkylanilines) synthesized using KI03 salt, the highest conductivity was obtained at P2EAn with a value of ^IxlO^Scm"1. polypyrrole was synthesized using iron (III) chloride salt. The highest yield was obtained at poly(N-methylaniline) (PNMAn) with a value of 87 %. The conducting composites were prepared by changing synthesis order of poly(alkylanilines) and polypyrrole. As a result of the formation of the composites, the conductivities of homopolymers were increased and it was determined that properties of composites were depend on synthesis order of polymers. Thermal degradation temperature (200°C) of PPy was observed to be higher than the other polymers and composites. From the Gouy balance magnetic measurements, it was found that the polymers and composites were bipolaron and polaron conducting mechanism. Polymerization and composite structures were supported by FTIR analyses. From UV-VIS spectra, the polymers were found to be in emeraldine structure. The morphological structures of polymers were clarifiedIV by Scanning Electron Microscopy (SEM). Intrinsic viscosity numbers of P2EAn, PNEAn, PNMAn and POT were obtained from viscosity measurements. The crystal structures of polymers were investigated by the powder X-Ray diffraction method. It was determined that structures of homopolymers and composites have amorphous regions with 5-12% and crystal regions with 88-95%. Science Code Key Words Page Number Adviser 405.02.01 Pyrrole, alkylanilines, composites. 116 Assoc. Prof. Dr. Bekir SARI