Dry-Sliding Friction and Wear of Powder-Metallurgy AA6061 Composites with Multiscale TiB2–SiC Reinforcement
Lubricants, cilt.14, sa.12, ss.1-20, 2026 (SCI-Expanded)
- Yayın Türü: Makale / Tam Makale
- Cilt numarası: 14 Sayı: 12
- Basım Tarihi: 2026
- Doi Numarası: 10.3390/lubricants14120449
- Dergi Adı: Lubricants
- Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED)
- Sayfa Sayıları: ss.1-20
- Gazi Üniversitesi Adresli: Evet
Özet
The dry-sliding friction and wear of AA6061 composites reinforced with micrometer-sized TiB2 and nanoscale SiC were investigated. The composites were produced by powder metallurgy, followed by hot extrusion, hot rolling, and T6 heat treatment. The first series contained 0, 2.5, 5, 10, or 15 wt.% TiB2. In the hybrid series, the TiB2 content was fixed at 10 wt.% and the nano-SiC content ranged from 0.25 to 2 wt.%. Microstructure, relative density, Brinell hardness, and transverse rupture strength were evaluated. Dry-sliding wear tests were conducted under normal loads of 5 and 15 N. At 5 N and a sliding distance of 300 m, the composite containing 10 wt.% TiB2 and 2 wt.% nano-SiC (S9) exhibited the lowest mean cumulative mass loss among the hybrid composites (0.0037 g), approximately 68% lower than that of unreinforced AA6061 under the same conditions. S9 also had the lowest reported coefficient-of-friction values (0.235–0.295). Scanning electron microscopy of the worn surfaces revealed grooves and localized smearing consistent with abrasive wear and a possible adhesive contribution. Crack-like features were also observed on the worn surface of S9.