Intergranular corrosion behavior of sensitized LPBF-Fabricated and wrought SS316L: Standardized assessment using ASTM A262 practices A and E


Puviyarasan M., Aniruddhan V., Rathinasuriyan C., chris A. B., Nagarajan L., Singh R. P., ...Daha Fazla

Journal of Materials Research and Technology, cilt.45, ss.6349-6358, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 45
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1016/j.jmrt.2026.10.107
  • Dergi Adı: Journal of Materials Research and Technology
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Compendex, INSPEC, Directory of Open Access Journals
  • Sayfa Sayıları: ss.6349-6358
  • Anahtar Kelimeler: ASTM A262, Intergranular corrosion, Laser powder bed fusion, Selective laser melting, Sensitization, SS316L
  • Gazi Üniversitesi Adresli: Hayır

Özet

Austenitic stainless steel 316L is a common material in engineering applications where corrosion protection is critical. It is known to be susceptible to intergranular corrosion (IGC) in the temperature range of 450 to 850 °C; this is caused by precipitation of chromium carbides and subsequent chromium depletion at the grain boundaries. The non-equilibrium microstructure produced by LPBF can alter the sensitization and corrosion behaviour, but there is not a complete consensus in published work. The present study compares LPBF-fabricated SS316L with commercially produced wrought SS316L after controlled sensitization treatment at 675 °C for 6 h following ASTM A262 Practices A and E, with the help of optical microscopy, SEM/EDS and XRD. The structure of both materials was mostly austenitic prior to the sensitization. The LPBF material showed melt pool boundaries, columnar grains, cellular substructure and porosity, while the commercial material was equiaxed structured. With practice A, the LPBF specimen demonstrated less severe grain-boundary ditching than the commercial specimen. The EDS observations suggested compositional variations in some regions of the boundaries, but the limited EDS data do not allow for quantitative measurements of chromium-depletion or the identification of the boundary precipitates. Practice E showed no visibly resolved intergranular cracking on the examined LPBF tensile surface, whereas intergranular cracking was observed in the commercial specimen. The corrosion rates of the LPBF SS316L and commercial SS316L were found to be 0.13 ± 0.02 mm/year and 0.50 ± 0.05 mm/year, respectively, by gravimetric analysis under the investigated condition. The results show that the LPBF material had a lower susceptibility to IGC than the commercial specimen under the sensitization and ASTM A262 conditions used. The findings should not be generalized to other sensitization histories or corrosion modes without further investigation.