Microstructural evolution, mechanical properties, corrosion behavior, and in vitro cytotoxicity of novel quaternary Ti-Nb-Ge-Zr alloys: A combined experimental and DFT study


Özdemir A., Güler E., Uğur G.

MATERIALS CHEMISTRY AND PHYSICS, cilt.373, ss.1-14, 2027 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 373
  • Basım Tarihi: 2027
  • Doi Numarası: 10.1016/j.matchemphys.2026.133386
  • Dergi Adı: MATERIALS CHEMISTRY AND PHYSICS
  • Derginin Tarandığı İndeksler: Academic Search Ultimate (EBSCO), Engineering Source (EBSCO), Scopus, Science Citation Index Expanded (SCI-EXPANDED), Chemical Abstracts Core, Chimica, Compendex, INSPEC
  • Sayfa Sayıları: ss.1-14
  • Gazi Üniversitesi Adresli: Evet

Özet

Two quaternary Ti-based alloys, Ti-7Nb-1.5Ge-3.5Zr and Ti-7Nb-1.5Ge-1Zr (wt.%), were produced by vacuum arc melting and characterized by EDXS, XRD, SEM, nanoindentation, potentiodynamic polarization in simulated body fluid (SBF) and the MTT cytotoxicity assay; the α phase was analyzed by density functional theory (DFT). Both alloys exhibit an as-cast Widmanstätten microstructure dominated by α with a minor β phase, which is more pronounced in the alloy with 3.5 wt% Zr. Nanoindentation yielded Young's moduli of 91.5 ± 3.9 GPa for Ti-7Nb-1.5Ge-3.5Zr and 95.6 ± 4.8 GPa for Ti-7Nb-1.5Ge-1Zr, lower than those reported for Ti-6Al-4V and low-Nb Ti–Nb alloys measured by the same technique but about three times the upper bound of cortical bone (10–30 GPa); the Zr-rich alloy is harder (2.68 vs 2.27 GPa). In SBF, both alloys exhibited low corrosion current densities (0.22 and 0.78 μA/cm2, respectively) and a passive region up to about 1 V vs. SCE. Their extracts were non-cytotoxic to L929 fibroblasts per ISO 10993-5 (cell viability 78.8 % and 73.5 %). Virtual-crystal DFT calculations indicate that the α phase of both alloys is mechanically stable with nearly identical elastic constants, so the property differences are attributed to the microstructure. Machine-learning-potential calculations on 96-atom random-alloy cells revealed no imaginary phonon modes, a stable hcp structure at 300 K and Young's moduli of 82–85 GPa, close to the measured values. Being free of Al and V and containing far less Nb than β-type Ti–Nb alloys, the alloys are of interest for further investigation as implant materials.