Effect of friction pressure on the properties of friction welded MA956 iron-based superalloy


ATEŞ H., Turker M., Kurt A.

MATERIALS & DESIGN, cilt.28, sa.3, ss.948-953, 2007 (SCI-Expanded)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 28 Sayı: 3
  • Basım Tarihi: 2007
  • Doi Numarası: 10.1016/j.matdes.2005.09.015
  • Dergi Adı: MATERIALS & DESIGN
  • Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED)
  • Sayfa Sayıları: ss.948-953
  • Anahtar Kelimeler: superalloys, MA956, friction welding, tensile strengths, hardness, FERRITIC ODS ALLOYS
  • Gazi Üniversitesi Adresli: Evet

Özet

Effect of friction pressure on the properties of friction welded hot rolled MA956 iron-based superalloy plate, produced by mechanical alloying, has been investigated. Joining processes were carried out by various friction welding parameters. Tensile strengths and hardness values of the weld interface were determined and the microstructure features of these samples were investigated. Optimum friction pressure for this material was determined. (c) 2005 Elsevier Ltd. All rights reserved.